YH-20 Resist Stripping Powder

Product Name:YH-20 Resist Stripping Powder
Solution Composition & Operating Parameters:
Concentration: 100 mL/L
Temperature: 45-55℃
Time: 1-3 min
Features and Applications:
1、Used to remove black film after nickel stripping on copper and iron substrates.
2、Does not attack copper and iron base materials.
Specification:
25KG woven bag